Boron magnesium ore dressing technology

Different beneficiation methods are used depending on the type of ore .

1. Boraxite type

Liaoning Liaoning Geological Central Laboratory had Houxianyu boron ore mine of this type of flotation pilot test carried out. The test ore adopts the middle ore remaining after hand selection, and the B2O3 content is 7% to 8%.

The flotation process control conditions are: the ore size is 3~0 mm, the I section grinding fineness -200 mesh accounts for 40%, the graded overflow concentration is 25%; the II section grinding fineness -200 mesh accounts for 75%, the graded overflow The flow concentration is 14%. The flotation slurry has a pH of 6.5 to 7.0 and a flotation temperature of about 40 °C.

Second, boehmite-magnetite-serpentine type

Such main mineral ore szaibelyite, a magnetic iron ore and serpentine. Boraxite is mainly fibrous, and the particle size of impregnation is generally 0.05 to 0.10 mm. The magnetite is impregnated with a particle size of 0.30 to 0.1 mm and is closely associated with the boehmite. A weak magnetic separation or weak magnetic separation-flotation combined process is employed. Figure 1 is Fengcheng, Liaoning

The stage of the second stage boron ore, the single weak magnetic separation process of magnetic separation.

Third, boehmite-carbonate type

The main minerals of Gaotaigou boron mine in Jilin Ji'an are boehmite, serpentine and magnesite . This type of boron ore can be either preferential or mixed flotation. See Figure 2 and Figure 3.

4. Boron magnesium petrochemical boron-magnesium iron ore-magnetite

Among such ores, boromagnesite, magnetite and serpentine are the main minerals. According to their specific magnetic susceptibility, a boron-magnesium iron concentrate can be obtained by using a weak magnetic-strong magnetic full magnetic separation process. The separation rate of ferro-boron can be determined by electric furnace smelting-pressure alkali hydrolysis method or direct reduction-magnetic separation method.

5. Uranium-boron-magnesium-iron-mineralized boehmite-magnetite type

The main useful elements of this type of deposit are iron, uranium , boron and magnesium. The Wengquangou uranium-iron-boron deposit in Liaoning belongs to this category. The ore dressing method steps are: selecting magnetite by wet weak magnetic field; recovering crystalline uranium ore by re-election, and obtaining boron-magnesium iron concentrate; obtaining boron concentrate by hydrocyclone classification, and the total selection process is as follows: Figure 4.



In addition, during the "Eighth Five-Year Plan" period, "Comprehensive utilization of boron-iron resources - research on the production of boron-containing pig iron and boron-rich slag in the bor furnace of boron ore" was carried out by the Northeast University and other units to separate the blast furnace iron and boron, and to activate the boron-rich slag. Significant progress has been made in key technologies such as boron, boron, uranium separation and uranium treatment.

Knock Box

Stainless steel coffee knock box ,different style and different size for you to choose.

Also can be powder coating finishing or mirror polishing or satin polishing .

Also welcome to combine the tamer, brush, Tamper Station, portafilter as one set.

Welcome to ask for any question or sent inquiry.

Knock box drawer,knock box,coffee ground waste box

Jiangmen Wellway Houseware Co.,Ltd , https://www.hkwellway.com

Posted on